C | Mn | Si | S | Ni | Fe | Others | |
Standard | ≤2.0 | ≤1.0 | ≤2.50 | ≤0.03 | ≥90 | ≤8.0 | ≤1.0 |
Typical | 0.59 | 0.07 | 1.50 | 0.004 | 94 | 0.021 |
Recommended Current (AC or DC)
Size (mm) | 2.5*300 | 3.2*350 | 4.0*400 | 5.0*400 |
Current(A) | 60-90 | 90-110 | 120-150 | 150-180 |
Attention
a. welding electrodes must be baked for 1 hour at the temperature of 80-120ºC before welding.
b. Hammering the welded seam to dispel stress around the welding region and to avoid cracking.
c. Large current should be avoided in cold welding for cast iron, so as to reduce impurities of base metal to penetrate the weld seam and to reduce the width of the weld zone, and then to improve the ability of crack-resistance and capability of machine processing of the weld seam.